Just wanted to say I was shocked and happy at how easy my plugs released from my molds. I don't have anything to compare it to but, All I did was pull the flange material away, then clean off the wax then I blew air around the outside of the plug and I could see it kind of fluttering in the mold. I flipped the mold over and gave it a few taps with my hand on the back of the mold and the plug fell right out.  I just hope I have enough to do everything I need. It was not cheap to get here.

Thanks,   Dennis
Reply
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
what is max temperature for easy lease? It's able to 90/100°C?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search