ideally you would build a jig that locks the metal inserts in a certain position during post curing.
If you need to worry about it or not depends a lot on what kind of accuracy you need and how your tempering oven looks like. if you have an oven with ramp control and you can increase the temp very slowly, you can basically chase the glass transition temperature of the resin in a way that it will always be higher than the temp in the oven and distortion should not be an issue with a part like this. If your setup is more simple then i would probably build a jig.
Nice looking parts!
|