Hy guys,

I have plug made from MDF that was CNC routed.

I've read that it's really hard to achieve gloss surface if MDF is not impregnated and "sealed" properly. It's hard for me to find products that are used for example in America and I have to take DIY approach. I figured that it might be possible to use polyurethane 2K varnish but diluted 20-30% so MDF can soak it easily.
Does anyone have similar experience? 

Also, I saw some DIY ovens made completely from support frame and MDF panels with rock wool between outer and inner panels. My plan is to build wooden frame, put 12 - 16mm MDF for outer shell, place rock wool around box from inside and than make smaller box that fits in from steel sheeting of aprox. 1-1.5mm thickness. I would make it so it opens from top side like a lid. I need curing temperatures of around 110-120°C (aprox. 250°F). Inner dimensions would be 160x70x50cm and I was thinking about 3 to 4 heaters of 1kW strength. 

Will this kind of build be ok to withstand those curing temperatures because I am afraid of oven catching fire? 

Also, I am looking for good PID controler with ramp and soak function so I can make proper curing cycle for pre-pregs. I've found some OMEGA controllers, but I am not quite sure what's good and what's not so please if you have suggestions feel free to write.



Replies
Dentex
D
Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)
Group: Forum Members
Posts: 42, Visits: 1.4K
Can someone please write me a list with all electric parts needed for oven? I understand that I need PID controller, silicone wiring for high temp, heating device and fan. 

I am considering Omega CN7500 or 7800, do I need something with it to function properly or it is ready to wire right out of box? Also does thermocouple comes with it or it needs to be purchased separately?
torsten Ker
t
Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)Supreme Being (629 reputation)
Group: Forum Members
Posts: 59, Visits: 278
Dentex - 10/16/2020 2:06:59 PM

as a ready to go one with 6 stages programable Temp and timer you may try the Inkbird ITC-310T-UK fro £40, it's ready wired.
That may be a good starter and can switch  13A.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dentex - 5 Years Ago
GT3 - 5 Years Ago
Rosta Spicl - 5 Years Ago
Dentex - 5 Years Ago
Rosta Spicl - 5 Years Ago
Dentex - 5 Years Ago
Dentex - 5 Years Ago
torstenker - 5 Years Ago
Hanaldo - 5 Years Ago
Dentex - 5 Years Ago
Hanaldo - 5 Years Ago
Dentex - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search