Can You Thicken Clear Epoxy Resin And Keep It Clear


Author
Message
dilligaf76
dilligaf76
Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)
Group: Forum Members
Posts: 49, Visits: 115
As per the title is there away of doing it? I have a few small problem areas that basically need filling but the resin is too thin to settle where I want it in one shot. I could thicken it to a paste by adding fillers of course but that would change the colour which I don't want, any ideas?
Reply
dilligaf76
dilligaf76
Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)
Group: Forum Members
Posts: 49, Visits: 115
oekmont - 8/3/2020 8:13:43 AM
There are liquid thickening agents, wich keep the resin clear. But if the resin is too thick, it won't release the trapped air any more.

Oh okay, what are these thickening agents called?

Edited 5 Years Ago by dilligaf76
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
dilligaf76 - 5 Years Ago
SleepingAwake - 5 Years Ago
dilligaf76 - 5 Years Ago
beliblisk - 5 Years Ago
oekmont - 5 Years Ago
dilligaf76 - 5 Years Ago
explorecomposites - 5 Years Ago
oekmont - 5 Years Ago
dilligaf76 - 5 Years Ago
oekmont - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search