By dilligaf76 - 7/31/2020 9:56:13 PM
As per the title is there away of doing it? I have a few small problem areas that basically need filling but the resin is too thin to settle where I want it in one shot. I could thicken it to a paste by adding fillers of course but that would change the colour which I don't want, any ideas?
|
By oekmont - 8/4/2020 3:09:46 AM
Well, I guess nobody's perfect. I have done it. The liquid stuff is not nearly as good as regular thixotroping additives, but it does it's job. However, you can't get the resin into a paste like consistency with it.
|
|