How much of each material do I need for carbon fiber hood


Author
Message
martinpastor
m
Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)
Group: Forum Members
Posts: 3, Visits: 6
Hello.
I watched the videos of the carbon fiber hood manufacturing but i want to know the approximate quantities of each of the materials that i would have to buy in order to acomplish it. Id like to manufacture some hoods so if I know the materilas for 1 i can approximate the ammount for about 10
Thank you
Replies
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Well are you making a bonnet for an Hyundai Getz or a Cadillac Coupe Devill? 

You basically just need to know the size of the part you are making. If it is a 1x1m part, then you will need 1sqm of material per layer. How many layers you do and of what materials is kind of up to you, you need to know what sort of properties you want the bonnet to have. The EC video is a pretty good starting point for a typical layup, but you might want to think about if its a street application maybe include some Kevlar in the layup for safety in a crash, or if it is a race application then perhaps it is a bit of a heavy layup and could be refined, etc. 
martinpastor
m
Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)
Group: Forum Members
Posts: 3, Visits: 6
Hanaldo - 7/28/2020 11:50:33 PM
Well are you making a bonnet for an Hyundai Getz or a Cadillac Coupe Devill? 

You basically just need to know the size of the part you are making. If it is a 1x1m part, then you will need 1sqm of material per layer. How many layers you do and of what materials is kind of up to you, you need to know what sort of properties you want the bonnet to have. The EC video is a pretty good starting point for a typical layup, but you might want to think about if its a street application maybe include some Kevlar in the layup for safety in a crash, or if it is a race application then perhaps it is a bit of a heavy layup and could be refined, etc. 

Thanks for the quick reply.
Im starting a workshop to manufacture parts such as hoods, mirror covers, lips, bodykits for cars. Therefore Id like to place an order to start this. but while watching the videos it wasnt clear how much of each material i would need. I just need an example of how much material you can use on an average hood, door ,etc to have an idea of what the first order should be to start manufacturing.

Greg
Greg
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 3, Visits: 15
martinpastor - 7/29/2020 1:42:23 AM
Hanaldo - 7/28/2020 11:50:33 PM
Well are you making a bonnet for an Hyundai Getz or a Cadillac Coupe Devill? 

You basically just need to know the size of the part you are making. If it is a 1x1m part, then you will need 1sqm of material per layer. How many layers you do and of what materials is kind of up to you, you need to know what sort of properties you want the bonnet to have. The EC video is a pretty good starting point for a typical layup, but you might want to think about if its a street application maybe include some Kevlar in the layup for safety in a crash, or if it is a race application then perhaps it is a bit of a heavy layup and could be refined, etc. 

Thanks for the quick reply.
Im starting a workshop to manufacture parts such as hoods, mirror covers, lips, bodykits for cars. Therefore Id like to place an order to start this. but while watching the videos it wasnt clear how much of each material i would need. I just need an example of how much material you can use on an average hood, door ,etc to have an idea of what the first order should be to start manufacturing.

Hi Martin, I was just browsing through this site and wanted to ask what part of the world you are in?  I don't have any experience in the area of composites but I've been doing a lot of research.  Was just thinking that if you happen to be within a reasonable distance we could share ideas and learn together.  Not to mention, potentially splitting some shipping costs from Easy Composites to the USA.  Based on what I've seen in EC's videos, these guys have a great line of products and a successful process for doing this sort of thing.  Anyway, I am typically between Houston Texas, or Lexington Kentucky, but currently in Kiev Ukraine during the current Pandemic of 2020.  My current goals are to build some replacement body panels for my Ferrari 360 project that I purchased with some collision damage.  I really only need a single fender & bumper, but I'd like to explore the possibility of doing both fenders (or maybe a 1 piece front end), a custom front bumper,  custom hood with NACA duct, and maybe try doing doors if I can work my skill level up to it.  For example, a new replacement fender is about $2,400usd (1,950 British Pound) from Europe + approx 20% on shipping.  And quality used parts are not so abundant at a reasonable price. (why does everyone always damage the left front???)

To anyone else who may be in the USA and interested to potentially join forces on shipping costs, please let me know.  I'd love to be able to save enough on shipping to be an EC customer for their complete line of products! (not only the ones which are super cheap to ship)

Sorry to ramble on... if you're in the USA, let's please connect and see if there is an opportunity to work together.  If you're outside the US, then certainly I wish you much success and let us know how you're progressing!

Best wishes,
Greg

_______________________________________________________________________________________________
"The slowest guy, in the slowest car, in the slowest run group is still having more fun than anyone sitting in the stands!"
2001 Ferrari 360 Modena (current project car)
2003 Porsche 911 (996 C2 in "arrest me" Guards Red, with the "lose your license" 6-speed manual transmission)
2008 Chevy 3500 Duramax

martinpastor
m
Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)Forum Guru (64 reputation)
Group: Forum Members
Posts: 3, Visits: 6
Greg - 8/2/2020 7:28:24 AM
martinpastor - 7/29/2020 1:42:23 AM
Hanaldo - 7/28/2020 11:50:33 PM
Well are you making a bonnet for an Hyundai Getz or a Cadillac Coupe Devill? 

You basically just need to know the size of the part you are making. If it is a 1x1m part, then you will need 1sqm of material per layer. How many layers you do and of what materials is kind of up to you, you need to know what sort of properties you want the bonnet to have. The EC video is a pretty good starting point for a typical layup, but you might want to think about if its a street application maybe include some Kevlar in the layup for safety in a crash, or if it is a race application then perhaps it is a bit of a heavy layup and could be refined, etc. 

Thanks for the quick reply.
Im starting a workshop to manufacture parts such as hoods, mirror covers, lips, bodykits for cars. Therefore Id like to place an order to start this. but while watching the videos it wasnt clear how much of each material i would need. I just need an example of how much material you can use on an average hood, door ,etc to have an idea of what the first order should be to start manufacturing.

Hi Martin, I was just browsing through this site and wanted to ask what part of the world you are in?  I don't have any experience in the area of composites but I've been doing a lot of research.  Was just thinking that if you happen to be within a reasonable distance we could share ideas and learn together.  Not to mention, potentially splitting some shipping costs from Easy Composites to the USA.  Based on what I've seen in EC's videos, these guys have a great line of products and a successful process for doing this sort of thing.  Anyway, I am typically between Houston Texas, or Lexington Kentucky, but currently in Kiev Ukraine during the current Pandemic of 2020.  My current goals are to build some replacement body panels for my Ferrari 360 project that I purchased with some collision damage.  I really only need a single fender & bumper, but I'd like to explore the possibility of doing both fenders (or maybe a 1 piece front end), a custom front bumper,  custom hood with NACA duct, and maybe try doing doors if I can work my skill level up to it.  For example, a new replacement fender is about $2,400usd (1,950 British Pound) from Europe + approx 20% on shipping.  And quality used parts are not so abundant at a reasonable price. (why does everyone always damage the left front???)

To anyone else who may be in the USA and interested to potentially join forces on shipping costs, please let me know.  I'd love to be able to save enough on shipping to be an EC customer for their complete line of products! (not only the ones which are super cheap to ship)

Sorry to ramble on... if you're in the USA, let's please connect and see if there is an opportunity to work together.  If you're outside the US, then certainly I wish you much success and let us know how you're progressing!

Best wishes,
Greg

Hi greg
Im from ecuador in southamerica. Im currently trying to find a forwarder in the UK to ship the products to Ecuador. Ferrari spare parts are very expensive so in your case I think this will be a great option. Anyway Im also trying to do some research on this topic because I studied mechanical engineering and we studied the composites topic  for a short time so definitely not enough for this projects.
I guess we will have many doubts on the learning process so we can help each other here.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
martinpastor - 6 Years Ago
Hanaldo - 6 Years Ago
martinpastor - 6 Years Ago
justGreg - 6 Years Ago
martinpastor - 6 Years Ago
Hanaldo - 6 Years Ago
justGreg - 6 Years Ago