Hello all,

Just ordered the XCR skinning kit, was wondering if it's possible to give it a matt finish? a dry carbon look, I kind of prefer that look, if so how do I best achieve that?
Just grind the shine away with mild sandpaper or 'roughly' sand it and spray it with matt varnish?

TIA
Reply
Gerrit72
G
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 3, Visits: 10
Warren (Staff) - 7/22/2020 12:05:43 PM
The only easy way to get a matt/satin finish is to spray with a lacquer.

Sanding it does not normally give an even matt look to the part.

Ok thanks, can I use a rattle spray can matt varnish or do I need something else?