Hi Matt,
The data sheet for your IN2-Infusion Resin gives the following schedule of times@temperatures for post curing:
24hrs @ room temperature 6hrs @ 40C 6hrs @ 50C 12hrs @ 60C
The Maximum Tg (glass transition?) temperature for the IN2 Infusion Resin is given as 94C - 100C for the slow cure mix. Is this the maximum temperature that this resin can be post cured to or should it be post cured to a lower temp? Ideally I would like to post cure to as high a temperature as possible as the parts are structural and will be subject to intense solar heating at times.
Can you suggest a post curing time@temp schedule beyond the one given above (say to 80 - 100C)? I understand the temperature ramp-up rate can be critical to the finished part's strength.
I am using both 5mm and 10mm thick closed cell PVC foam core material in my laminates - what temperature can this foam board take before it starts to degrade - can it withstand the higher post curing temperatures?
Thanks,
Phil.
|