Just to add to point 1, if you're using EC's GC50 for your in-mould coating, you'll get much better cosmetic results from spraying it into the mould. Applying by brush is likely to leave cured ridge lines and brush marks that''ll likely distort to the clarity of the cured part, as the fabric won't be able to lay flat against the coating when infused
If this isn't a practical option for you, then you might get better results from leaving out the in-mould coating and looking to have a post-production clear coating applied, especially as and when you progress onto bigger items like bonnets etc.
Stick with it, as there's always a learning curve to navigate and you'll eventually get your techniques nailed down
|