VAC CAST EPOXY CASTING RESIN


Author
Message
Moreno Marchetti
Moreno Marchetti
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 5, Visits: 15
We are an Italian company which sells and installs natural stones, marbles.
We would like to receive a feedback from you, because our Indian marble supplier used your expoxy resin on the surface of Rainforest Green Marble with brushed finish.
We have installed this marble inside a private pool and we would like to be sure that your product doesn't affect marble under sun-light or in contact with pool water!!

Have you ever had similar experience?

Waiting for your kind reply


societàdellapietra srl
Via Cellini, 140
60019 Senigallia (AN) Italy
P.I. 02104010422
Tel. 071.7931020
wwww.societadellapietra.com
Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Are you sure it was the Vac Cast epoxy?  This product: Vac Cast Epoxy Casting Resin

Or did you mean our GlassCast such as GlassCast 3?

If it was the latter, GlassCast 3 is not rated for permanent underwater use so we have no data to know exactly how long it may last or how it may degrade. Fully Cured epoxy is generally waterproof so I would expect it would be fine initially but long term it may not have the durability you need. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Moreno Marchetti
Moreno Marchetti
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 5, Visits: 15
Warren (Staff) - 7/7/2020 4:35:49 PM
Are you sure it was the Vac Cast epoxy?  This product: Vac Cast Epoxy Casting Resin

Or did you mean our GlassCast such as GlassCast 3?

If it was the latter, GlassCast 3 is not rated for permanent underwater use so we have no data to know exactly how long it may last or how it may degrade. Fully Cured epoxy is generally waterproof so I would expect it would be fine initially but long term it may not have the durability you need. 

Thanks Warren.
Yes, it was Vac Cast Epoxy Casting Resin! Sad

Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I have no idea why they would use that resin for that application. Unfortunately there is no data and no real world experience with using VacCast in that way so I am not sure how it would last. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Moreno Marchetti
Moreno Marchetti
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 5, Visits: 15
Warren (Staff) - 7/8/2020 8:12:18 AM
I have no idea why they would use that resin for that application. Unfortunately there is no data and no real world experience with using VacCast in that way so I am not sure how it would last. 

Our Indian marble supplier told me that they always use your Epoxy casting resin on brushed marbles....... Sad
Which are the properties of this product for a marble?

Thanks for your availability
 

Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Are you sure you mean VacCast?  the resin is grey in colour and it would seem odd to cover a green marble slab in a grey resin.... Or am I misunderstanding you?

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Moreno Marchetti
Moreno Marchetti
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 5, Visits: 15
Yes, I'm sure.They send us a photo of the product
Actually they told us it is clear and transparent, but we have some doubts beacuse it seems to add colour to the marble surface??!!




Moreno Marchetti
Moreno Marchetti
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 5, Visits: 15
Moreno Marchetti - 7/9/2020 9:07:41 AM
Yes, I'm sure.They send us a photo of the product
Actually they told us it is clear and transparent, but we have some doubts beacuse it seems to add colour to the marble surface??!!




What do you suggest?
To try and take away it, with the help of some other specific product of yours, before covering the marble with pool water?
Thanks

Hanaldo
Hanaldo
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I feel like there has to be some confusion or something is getting lost in translation here... VacCast is an aluminium filled epoxy. It is dark grey and completely opaque. It is so unsuitable for this application that I just can't fathom that anyone would have thought it would be suitable... and if they are telling you that it is clear, then either they are blatantly lying, or they are talking about a different product.
Edited 6 Years Ago by Hanaldo
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search