Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
When I first started playing with infusion, I experimented with the stretchy films and it was a nightmare for all the reasons mentioned. Worst was that the infusion would seem ok then suddenly the bag would burst. I found out the bag was going into the open side of the silicone connector then starting to stretch to try and fill the void under the silicone and would keep stretching until it burst. Not to mention the bag stretching over cut mesh edges and slowly bursting and leaking there during the infusion!
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|