Afternoon all
Can anyone point me in the direction or know where I may get hold of a small amount of strechlon bagging material ?
I have a job coming up that I don't do very often but do use the film , and I have run out 🙄

Cheers tony
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Rich (Staff) - 5/29/2020 9:06:35 AM
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

Ha! Both products I bought about 5m each of, and still have both sitting mostly untouched on the rack... I can understand why they got dropped Smile

Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Rich (Staff) - 5/29/2020 9:06:35 AM
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

Why did you drop it? With a 500% stretchability it seems to be great stuff. There is even a version that appears to be able to withstand oven temperatures. What are the downsides? 

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Steve Broad - 6/9/2020 12:57:37 PM
Rich (Staff) - 5/29/2020 9:06:35 AM
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

Why did you drop it? With a 500% stretchability it seems to be great stuff. There is even a version that appears to be able to withstand oven temperatures. What are the downsides? 

It's not as useful as it promises. If you know how to make a vacuum bag with regular bagging film, then those films are tougher and much easier to work with. Strechlon sticks to epoxy, it punctures very very easily, it doesn't stick well to bagging tapes, and it has various issues with infusion etc. About the only thing I have had much use for it with is vacuum bonding.


Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 6/9/2020 1:26:28 PM
Steve Broad - 6/9/2020 12:57:37 PM
Rich (Staff) - 5/29/2020 9:06:35 AM
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

Why did you drop it? With a 500% stretchability it seems to be great stuff. There is even a version that appears to be able to withstand oven temperatures. What are the downsides? 

It's not as useful as it promises. If you know how to make a vacuum bag with regular bagging film, then those films are tougher and much easier to work with. Strechlon sticks to epoxy, it punctures very very easily, it doesn't stick well to bagging tapes, and it has various issues with infusion etc. About the only thing I have had much use for it with is vacuum bonding.


So, no real issues, then :-)

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Steve Broad - 6/9/2020 4:19:40 PM
Hanaldo - 6/9/2020 1:26:28 PM
Steve Broad - 6/9/2020 12:57:37 PM
Rich (Staff) - 5/29/2020 9:06:35 AM
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

Why did you drop it? With a 500% stretchability it seems to be great stuff. There is even a version that appears to be able to withstand oven temperatures. What are the downsides? 

It's not as useful as it promises. If you know how to make a vacuum bag with regular bagging film, then those films are tougher and much easier to work with. Strechlon sticks to epoxy, it punctures very very easily, it doesn't stick well to bagging tapes, and it has various issues with infusion etc. About the only thing I have had much use for it with is vacuum bonding.


So, no real issues, then :-)

No not at all, it is a commercial product used by professionals all over the world for a reason. If it was inherently flawed with defects then it would not be. I just found it not very reliable, and not as useful as a basically infinitely stretchy bag seems on paper, and so never bought any more of it. I'd say a lot of EC's customers came to the same conclusion, and it got dropped from the line-up.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Big Tee Racing - 5 Years Ago
     Try fibreglast
mporta71 - 5 Years Ago
Big Tee Racing - 5 Years Ago
             No, in the US
mporta71 - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
Big Tee Racing - 5 Years Ago
Hanaldo - 5 Years Ago
Rich (Staff) - 5 Years Ago
Hanaldo - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
                         So, no real issues, then :-)
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
explorecomposites - 5 Years Ago
BoB_from_jungle - 5 Years Ago
Hanaldo - 5 Years Ago
Rich (Staff) - 5 Years Ago
Warren (Staff) - 5 Years Ago
BoB_from_jungle - 5 Years Ago
Hanaldo - 5 Years Ago
Steve Broad - 5 Years Ago
SleepingAwake - 5 Years Ago
Steve Broad - 5 Years Ago
SleepingAwake - 5 Years Ago
Hanaldo - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
Hanaldo - 5 Years Ago
oekmont - 5 Years Ago
             Which bagging film are you using?
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago
Hanaldo - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search