the correct resin to join timber


Author
Message
jonnyseka
j
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 12
Long story short
the Oak veneer has peeled of my external oak doors so ive sanded it off and i'm planning on using epoxy resin too attach(glue)  8mm strips of oak to the existing doors. what resin would you recomend

cheers

J
Replies
jonnyseka
j
Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)Junior Member (20 reputation)
Group: Forum Members
Posts: 3, Visits: 12
Warren (Staff) - 5/20/2020 12:14:23 PM
XCR Epoxy Coating resin is slightly thicker than EL2 making it a bit easier to get a nice even coat over wood work.  It is commonly used over wood for protection and decorative purposes.  It's also a bit quicker and easier to use than EL2 as you can overcoat within a couple of hours and it is easily sanded and polished back up if there are any surface blemishes to fix.

brilliant,  this is all starting to make sense now,  when using  thickener   what is the difference/ pros cons between  Glass Bubbles (Microspheres) and Fumed Silica Thixotropic Powder

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
jonnyseka - 5/20/2020 12:39:18 PM
Warren (Staff) - 5/20/2020 12:14:23 PM
XCR Epoxy Coating resin is slightly thicker than EL2 making it a bit easier to get a nice even coat over wood work.  It is commonly used over wood for protection and decorative purposes.  It's also a bit quicker and easier to use than EL2 as you can overcoat within a couple of hours and it is easily sanded and polished back up if there are any surface blemishes to fix.

brilliant,  this is all starting to make sense now,  when using  thickener   what is the difference/ pros cons between  Glass Bubbles (Microspheres) and Fumed Silica Thixotropic Powder

Glass bubbles are used to reduce the density of the resin, thickening it while also making it much easier to sand. Great for making epoxy fairing pastes. 

Fumed silica is a thixotropic additive, which is different to thickness. It changes the behaviour of the resin under shear stress, meaning that when it is just sitting it will be very thick and not sag, but when you are brushing it or moving it, it will be much thinner and still easy to move around. If you've ever worked with gelcoat, gelcoats are a thixotropic substance. As is honey.

You sometimes might want to combine the two to get the properties you want. Glass bubbles on their own will make a nice thick paste, but it won't be thixotropic and so might still sag if used in thick sections of a vertical. It also makes for a relatively brittle resin, thanks to its low density. While fumed silica is great for making pastes that won't sag, but because it is derived from quartz it also makes the substance extremely difficult to sand. 