			            Generally speaking, your mould would be made as a solid closed vent item.  In terms of lay up, you will need some overlap to give neat edges to trim back to. If you use pre-preg or a stabilised fabric like our ProFinish carbon cloth, you can cut the edges quite cleanly so you would only need an overlap of a mm or so to give something to sand smooth against.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |