You really don't need a second resin inlet. This is a fairly easy part. I have done parts the size of half a car with only one inlet. A second one will only make it more difficult to solve the real problem. If your flow mesh punctures the bag, I would suggest to get better bagging material. The switch to pa/pe/pa was one of the best decisions I've ever made.
|