MGS Hexiom L285 is a good product, I've used it before because it is one of very few resins that are approved for use on gliders. The blue colour is a tint they use so you can see it has been mixed properly. Once mixed, it is a very light shade of blue that you won't be able to see on carbon unless it is extremely resin rich.
|