Hello,
what are the ways to extend the pot life of polyester resin (if possible)?

Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Epoxy is harder to hand laminate with than polyester, for sure. 

It sounds like you are mixing your batches too big? Only mix what you can use within the pot-life. As you get experience, you will learn to work faster and be able to mix larger batches. I started off struggling to get 500g on the job before it started to gel. These days I have no worries mixing 2kg on a 40° day and getting it all on in 5 minutes. But start slow, give yourself more time by doing more mixing.
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 5/4/2020 1:42:34 AM
Epoxy is harder to hand laminate with than polyester, for sure. 

It sounds like you are mixing your batches too big? Only mix what you can use within the pot-life. As you get experience, you will learn to work faster and be able to mix larger batches. I started off struggling to get 500g on the job before it started to gel. These days I have no worries mixing 2kg on a 40° day and getting it all on in 5 minutes. But start slow, give yourself more time by doing more mixing.

2kgs in 5 mins? How many arms do you have? :-))

You are right... I need more practice with smaller parts and especially smaller batches.
What is your preferred tool to spread the resin? Brush, roller, squeegee etc.?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
oekmont - 5 Years Ago
Hanaldo - 5 Years Ago
oekmont - 5 Years Ago
mporta71 - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search