Hey People,,

Here's a quick one thats hopefully straightforward?

My problem is, I am making a  plug and getting ready to take the mould. The plug is pretty much a rectangular cube which I'm gonna do in 2 sections, 3 sides of the box per mould.

Now to make the mould I've stuck on some corrugated card to act as flanges that block off the parts I do not want to use yet. So the question is, how do i stop gelcoat getting between the card and the plug? There's very little room to use modeling clay as it will get in the way of the defined corner.. Do I pull the card away a little and then fill the gap with clay, just behind the corner?

Or do  I use nothing at all and hold the card in place (its stuck on with double sided tape, i'd just be holding it to stop it flexing too much) whilst applying the gelcoat, using any lines created as guide lines when I trim the part??

I can post any pics if needed, just let me know! Smile

Thanks for your help!

Rob

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The only problem with tape is movement.  If the flange has adequate support, that may not be an issue.  Hot melt glue is good in that respect as you can build nice fillets of it to keep the flange straight. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
robenergy - 5 Years Ago
robenergy - 5 Years Ago
beliblisk - 5 Years Ago
robenergy - 5 Years Ago
robenergy - 5 Years Ago
Hanaldo - 5 Years Ago
robenergy - 5 Years Ago
Hanaldo - 5 Years Ago
robenergy - 5 Years Ago
Warren (Staff) - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search