+x Hanaldo - 4/25/2020 3:36:05 PMDefinitely hot melt glue. I use 3mm coreflute, and glue the flanges on from the back side of the flange. Then seal the gap with filleting wax.I remember the struggle of using plasticine/clay. Filleting wax changed my life, I'll never go back!