Hi all, 

I have a question regarding making moulds from mdf or oak. I cnc milled 2 moulds, one from MDF and one from oak. Moulds are for bike helmet I want to make.
Can you recommend what final layers should I put on mould? What couloring or something like that?

I already tried to put some colors but mould got ruined because carbon with epoxy resin glued to it.

Please any help and I will be grateful.
Reply
kosak95
k
Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)Supreme Being (147 reputation)
Group: Forum Members
Posts: 14, Visits: 518
Chris Rogers - 4/25/2020 6:31:10 PM
I agree with Lester.  You need to seal the wood before you can do anything.  You can release off a primer surface or even well resin-coated wood but it still takes some work.  MDF will work fine for composites molds provided you don't expect too much.  Oak may crack in thick sections and be unstable because of the grain - but I've never tried it!  

Here's an article I wrote about using MDF for molds:  https://explorecomposites.com/articles/tooling/using-mdf-for-composites-tooling/

Thanks for reply. I read your article and find it helpful.
After you sand first layer of epoxy ? Do you add extra layer of epoxy onto it? Or one is enough? And what kind of paint you put on epoxy then?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
kosak95 - 5 Years Ago
Warren (Staff) - 5 Years Ago
kosak95 - 5 Years Ago
SleepingAwake - 5 Years Ago
explorecomposites - 5 Years Ago
kosak95 - 5 Years Ago
explorecomposites - 5 Years Ago
kosak95 - 5 Years Ago
SleepingAwake - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search