By kosak95 - 4/21/2020 8:02:02 AM
Hi all,
I have a question regarding making moulds from mdf or oak. I cnc milled 2 moulds, one from MDF and one from oak. Moulds are for bike helmet I want to make. Can you recommend what final layers should I put on mould? What couloring or something like that?
I already tried to put some colors but mould got ruined because carbon with epoxy resin glued to it.
Please any help and I will be grateful.
|
By SleepingAwake - 5/8/2020 11:41:29 AM
you want the epoxy just to seal the wood. apply generously and at the end of the pot live wipe away all excess resin with a shop towel.
once it is sealed you can continue with 2k-paint. Usually a wooden surface will not leave you with an acceptable finish with paint and no sealer.
|
|