Group: Administrators
Posts: 167,
Visits: 4.6K
|
We've experimented with the Green Hybrid fabric and it works reasonably well with the XC110 resin, the issue is that it becomes incredibly dark, so much so that in most lights it looks black; we can look at custom PrePregs potentially but generally its based on full roll quantities so you're looking at around 50 to 100m to run it through and its a lot of material if it doesn't go as planned. It'd be interesting to see the Composites Evolution ones once cured though as the metallic filament may be brighter than the dyed filaments in our hybrid range.
Have you used the EvoPreg materials Steve - if so what are they like?
|