Lenny
Lenny
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 58
Do you supply pre-preg in any others colours than black ?
I would like to some red (as per the cloth/fabric).
Please advise.
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pre-preg in red
Lenny
-
6 Years Ago
Unfortunately we are not able to get hold of any other pre-pregs in different colours. I would imagine they are very rare if you can find it at all.
Warren (Staff)
-
6 Years Ago
https://compositesevolution.com/news/composites-evolution-introduces-decorative-coloured-carbon-prepregs/
Steve Broad
-
6 Years Ago
Thanks all, will check out the link.
Lenny
-
6 Years Ago
We've experimented with the Green Hybrid fabric and it works reasonably well with the XC110 resin, the issue is that it becomes incredibly dark, so much so that in most lights it looks black; we can....
Rich (Staff)
-
6 Years Ago
Hi Rich No, I found it a few months ago whilst doing a bit of research :-)
Steve Broad
-
6 Years Ago
Thanks Steve, I was trying to figure out if its actually available to purchase yet but cannot tell from the website, I'll see about contacting them as it would certainly be interesting to see how the...
Rich (Staff)
-
6 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search