Hey all, I need help with a few things, I am manufacturing Carbon fiber parts for the honda CBR600rr and my customers continue asking me to make these complex parts and I hate turning money away. So here it goes.

One is a small corner piece with awkard tabs for mounting it:





The second issue I am having is how to fabricat the interior of the stator cover. It will be holding hot oil too so it has to be durable.



Lastly I would like advice on what to use as an alternative to the factory's injected screw threads I guess you can call them. They are basically the threads on the back of the fairings/body panels that your small screws go into ..idk how else to explain it and cant find a picture online anywhere.

Thanks in advance!
Warren
Warren
Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)Supreme Being (3.5K reputation)
Group: Administrators
Posts: 214, Visits: 783
clip detail can be done by casting then bonding in the cast part.  Youd make a silicone mould then use polyurethane fast cast to make the part.  can also be pigmented to black or whatever.  You can get a casting kit at EC.

For threads, you can use "bighead" fasteners if there is space or use "u clips" with a thread:
http://www.taiwantrade.com.tw/resources/member/115216/productcatalog/c01fbccb-edf2-406b-b98c-1e406a56314f_HW001.JPG
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search