Best face masks for steryne ?


Author
Message
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
What mask will you recommend for steryne smell?
Replies
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
you want a paint spraying mask, something like this

https://www.screwfix.com/p/trend-stealth-half-mask-p3r/346fh



Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
scottracing - 2/29/2020 10:28:27 PM
you want a paint spraying mask, something like this

https://www.screwfix.com/p/trend-stealth-half-mask-p3r/346fh



Wait this is only a particle filter isn't it? You need a particle filter and a filter to remove VOC's.
I like the masks from Sundström, others prefer 3M.

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Lester Populaire - 3/1/2020 9:10:29 AM
scottracing - 2/29/2020 10:28:27 PM
you want a paint spraying mask, something like this

https://www.screwfix.com/p/trend-stealth-half-mask-p3r/346fh



Wait this is only a particle filter isn't it? You need a particle filter and a filter to remove VOC's.
I like the masks from Sundström, others prefer 3M.


yeah i would go for an air fed 3M, but they are asking to remove the smell.
As long as they arent in a confined space using large amounts of resin any half decent maskwould do.

Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
scottracing - 3/1/2020 9:49:18 PM
Lester Populaire - 3/1/2020 9:10:29 AM
scottracing - 2/29/2020 10:28:27 PM
you want a paint spraying mask, something like this

https://www.screwfix.com/p/trend-stealth-half-mask-p3r/346fh



Wait this is only a particle filter isn't it? You need a particle filter and a filter to remove VOC's.
I like the masks from Sundström, others prefer 3M.


yeah i would go for an air fed 3M, but they are asking to remove the smell.
As long as they arent in a confined space using large amounts of resin any half decent maskwould do.

Hi, you need and should always wear a mask with A2 filter types (volatile solvents). The one listed above is not suitable, it just filters out dust.
(Dust filtering is P1, P2, P3 - the higher the P index, the most effective the filter is able to filter smaller particles).
The best would be combination of A2 + P3.
If you check the 3M website you can check all the combinations.



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search