Talk Composites - The Forum for Advanced Composites

Best face masks for steryne ?

http://www.talkcomposites.com/Topic34948.aspx

By Classicarbon - 2/29/2020 1:04:38 PM

What mask will you recommend for steryne smell?
By mporta71 - 4/25/2020 9:16:19 PM

scottracing - 3/1/2020 9:49:18 PM
Lester Populaire - 3/1/2020 9:10:29 AM
scottracing - 2/29/2020 10:28:27 PM
you want a paint spraying mask, something like this

https://www.screwfix.com/p/trend-stealth-half-mask-p3r/346fh



Wait this is only a particle filter isn't it? You need a particle filter and a filter to remove VOC's.
I like the masks from Sundström, others prefer 3M.


yeah i would go for an air fed 3M, but they are asking to remove the smell.
As long as they arent in a confined space using large amounts of resin any half decent maskwould do.

Hi, you need and should always wear a mask with A2 filter types (volatile solvents). The one listed above is not suitable, it just filters out dust.
(Dust filtering is P1, P2, P3 - the higher the P index, the most effective the filter is able to filter smaller particles).
The best would be combination of A2 + P3.
If you check the 3M website you can check all the combinations.