How do I secure the best possible bonding between epoxy and high modulus aramid fibres.

Is it necessary to remove the fiber spin finish before laminating or pultrusion.

Thanks for your feed back.

Flemming
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)Composites Expert (Staff) (12K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Flemming,

Sorry for the delay in getting back to you. Aramid fibres designed for composites use should already be prepared ready for epoxy bonding. I assume you're referring to a fibre that we don't supply (high modulus aramid) so I would recommend you speak to your manufacturer/supplier and ensure that the aramid is suitable for epoxy bonding to be sure.

Best regards, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search