Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi Doug,
Is there some reason why you plan to use resin rather than concrete into these holes? I guess it’s because the posts are quite a snug fit into the holes so it’s more of a bonding function than concrete could provide.
There are a number of our resins that could be used but I’d need to check the environmental conditions with you first. Can the work area be kept dry throughout the cure (up to 24hrs) and be maintained at a temperature of >15C throughout?
If you can confirm, I’ll make some recommendations.
All the best, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|