Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Do a test mix of each component. The high filler content and styrene base for the Uni-mould system means it can dry up and degrade quite quickly hence the short shelf life. If it has been kept ok then the chances are it will still be usable.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|