Shelf life of uni-mold system


Author
Message
Hansson43
H
Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)Supreme Being (234 reputation)
Group: Forum Members
Posts: 23, Visits: 2.1K
Hi, haven’t been able to use the uni mold system I ordered in september 2019 because life I guess, and I have seen that the shelf life is 3 months. I haven’t open the cans. Will they still be to good use or do I need to order a new batch ?
Thank you