Hi Brian,
I see, that's much more clear now. I did consider the P6 but wondered how much 'give' this block would need. If it's just a static compressive load then Xencast P6 would also be a good option. P6 is definitely a more 'rigid' system but it does have more flexural strength than than a conventional Fast Cast type PU, such as our Xencast P2. It's worth pointing out that to get the full benefit from the toughened P6 system it would need to be degassed. I'm not sure if you have those facilities? - Degassing is not *essential* but it does improve the toughness of the casting and realise the full potential of the P6 resin system.
Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|