Hi everyone, 

I am just starting into the hobby of mould making and duplicating of car parts. I have done some research on mould making and products but I haven't been able to find an answer to the issues that I have with the car part that I am wanting to duplicate. I am wanting to duplicate a Toyota shift bezel for a mid 80's Toyota that is no longer produced. 

I know I will have to do a two part mold. I will have to back fill the shifter with clay, cast one side, then remove the clay, and cast the other side,. 

The issue that I am stuck with are these small clips that are on the underside of the bezel that keeps the shifter boot in place. How do I go about making a mold with these? As I see it if I pour the silicon mold material in that they will tear when I remove the bezel. 

Any ideas?





Reply
Hojo
Hojo
Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)Supreme Being (289 reputation)
Group: Forum Members
Posts: 31, Visits: 957
3D print and glue the clips on after. You could mould the clip potentially, but a ot of extra effort. 3D printing is typically the way to go on this