I’m curious if the quality of a tools surface can cause issues on the parts surface or cause resin flowing issues. For our tool we’re using 10lb urethane foam that’s been mulled and then poly primer sealed and surface to 320g. Then release applied and then infused a part. This tool surface is in no way close to a gel coated polished out tool. Curious if this type of surface would cause any issues to the parts surface or the way resin does across the surface. I know the part will come out more a matte finish, it i’m curious if anyone knows if this type of tool surface is not ideal and no matter what is done you will never be able to get a flawless part out of it.
|