Hi all, just wonder if anyone have some advice regarding Frekote 700, the problem is that we can´t control that we have release agent all over the tool, is there any way that you can control the coat, i mean maybe with UV-light or is there any coloragent you can apply. We have some complex tools and just the smallest of spots without frekote makes it stuck.
Thanks/Chris 

Reply
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Chrill - 12/5/2019 5:55:58 AM
Hi all, just wonder if anyone have some advice regarding Frekote 700, the problem is that we can´t control that we have release agent all over the tool, is there any way that you can control the coat, i mean maybe with UV-light or is there any coloragent you can apply. We have some complex tools and just the smallest of spots without frekote makes it stuck.
Thanks/Chris 

Get better laminators ! If you can't release a mould shouldn't be doing the job !
If you have really tight corners brush all corners with an artist's brush then damp lint free cloth on all surfaces working from top to bottom.
Bit like the joke that bad window cleaners only do round windows