Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Same as above for the coffee table resin. These resins are quite hard for resins, but they are not as hard as a lot of items that they will come into contact with - which means scratches.
Also with a coffee table, often the bigger issue is people put a hot cup of coffee down on the surface. This is a big no no. Even a warm cup of coffee may cause issues - anything over about 50-60 degrees will mark the resin. Nothing can be done about this other than to use a coaster or protect the surface somehow.
|