Xpreg xc110


Author
Message
Thomb
Thomb
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 23, Visits: 656
Hi all,

Im still having some problems with the xpreg in gelcoat moulds. When i use aluminium moulds all is good. When i use the high temp gelcoat moulds i always get a dry finish on the mould side. I tried some longer times and diffrent temperatures but i keep getting these results. I only use breather underneath the mould but that always worked for me and only the bag where it it packed in to press on the carbon. Does anyone have a clue what could be it or what i can try?







Edited 6 Years Ago by Thomb
Reply
Thomb
Thomb
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 23, Visits: 656
So a little update,

I tried various temps and soaks but the end result is the same, always these dry finishes. I tired a little 5x5cm piece same 2 layers in the same mould and this comes out perfectly. What i am doing wrong? already tried with perforated release film and peelply on the back but same results.

Result with small carbon layup in same mould with same times:


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Thomb - 6 Years Ago
SleepingAwake - 6 Years Ago
Shaneer22 - 6 Years Ago
Hanaldo - 6 Years Ago
Shaneer22 - 6 Years Ago
Thomb - 6 Years Ago
Thomb - 5 Years Ago
explorecomposites - 5 Years Ago
Hanaldo - 5 Years Ago
                 Yes same prepreg same mould same times.
Thomb - 5 Years Ago
explorecomposites - 5 Years Ago
carbon man - 5 Years Ago
             Yes i use autoclave now and all good