Hello guys,

I have this project i need some help with please.
I bought this longboard that is made for people of 65kg and im 85kg. It was intentionaly so after applying the carbon fiber im gonna have a lighter and cooler board.

Image result for pantheon trip 7 ply

Im thinking on applying 3 layers of unidirectional carbon fiber as i just need more strenght verticaly. Im not vaccuum bagging.

My plan is:
1 - Sand the bottom of the board to the raw wood so the carbon fiber sticks to it.
2 - Apply a first layer of EL2 Epoxy Laminating Resin 500g FAST (Can i do this or its necessary that i apply a XCR Black Epoxy Basecoat 500g?)
3 - After X time apply the first layer of carbon fiber (How long I should wait to apply the first layer and between the 2 and 3 layers?)
4 - Apply the final laer of epoxy.

What carbon fiber do you guys reccomend i use, the 250gsm or the 100gsm?

These are the itens im planning on buying
Thanks for the help.

Mateus Cavinato.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search