Dear all. I am facing problems with IN2 Infusion Epoxy resin pigmented with Dust grey WS26121A. Applying wet laid process and after 24h, the epoxy has not cured. The weight of the components is the following: 125g (IN2 infusion epoxy), 37,5g (AT30 slow), 17,5g (dust grey WS26121A). I made trials with the same epoxy with TiO2 to obtain white coloured sheet and the curing was correct after 15h. Can somebody give me an explanation about this problem? I would appreciate a prompt answer as I have to produce some prototypes as soon as possible. Thanks to all. Andreu





Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
IN2 can achieve over 80C with a post cure.  Post cure the finished part with one of the cycles in the TDS and you should be fine with it being at 70C all day long. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search