Gelcoat scratch removal?


Author
Message
Robert72
R
Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)Supreme Being (519 reputation)
Group: Forum Members
Posts: 57, Visits: 151
Hello all.  I have made a mould using the Uni-Mould system.  The pattern was finished with Pattern-Coat High-Gloss, and had some scratches (I had started with 80 grit).  But I made the mould anyway and the scratches, as expected came through.  So the scratches on the mould were now male scratches and easier to remove.  So this time I started with 400 grit wet (wet, circular motion, 3 sessions), followed by 800 (wet, circular motion, 2 sessions), followed by 1200 (wet, circular motion, 2 sessions).  Attempted polish with Topfinish2 and medium/soft blue pad in DeWalt polisher, but ended up with deep scratches.  Also have attempted NW1 cutting compound with medium/hard orange pad, still no cigar.

I have ordered 1500 and 200 grit, I will start again at 800 grit and go through 1200, 1500 then 2000. And then probably NW1.

Any other suggestions? You can clearly see the scratches in the pictures, the phone camera picks them up really well. In the third picture, you can see how rough the surface is in the light section. One problem is that the entire mould is concave, but my pads are flat.  Are there hemispherice pads available anywhere?








Reply
wayne livesey
wayne livesey
Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)Forum Member (33 reputation)
Group: Forum Members
Posts: 4, Visits: 27
Robert72 - 10/6/2019 1:20:50 PM
Hello all.  I have made a mould using the Uni-Mould system.  The pattern was finished with Pattern-Coat High-Gloss, and had some scratches (I had started with 80 grit).  But I made the mould anyway and the scratches, as expected came through.  So the scratches on the mould were now male scratches and easier to remove.  So this time I started with 400 grit wet (wet, circular motion, 3 sessions), followed by 800 (wet, circular motion, 2 sessions), followed by 1200 (wet, circular motion, 2 sessions).  Attempted polish with Topfinish2 and medium/soft blue pad in DeWalt polisher, but ended up with deep scratches.  Also have attempted NW1 cutting compound with medium/hard orange pad, still no cigar.

I have ordered 1500 and 200 grit, I will start again at 800 grit and go through 1200, 1500 then 2000. And then probably NW1.

Any other suggestions? You can clearly see the scratches in the pictures, the phone camera picks them up really well. In the third picture, you can see how rough the surface is in the light section. One problem is that the entire mould is concave, but my pads are flat.  Are there hemispherice pads available anywhere?








All weekend I have tried everything to polish this glasscast 3 up I have been through every grit up to 3000 I've tried wet, dry and nw1 compound you just can't get it to look like glass once you have sanded it I'm going to call them tomorrow AGAIN about this issue in the videos I looks like it will just polish to a glass finish. I have literally waisted my whole weekend sanding and polishing it just don't come up like glass I'm so disappointed with this glass cast 3. I've even been and spent £300 on a decent polisher but still no luck I think it's a myth that once sanded you can get it back like a piece of glass. I will say that the higher the grit did make a difference but not to look how it should. I'm fuming I could rant on all night 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Robert72 - 6 Years Ago
wayne livesey - 6 Years Ago
wayne livesey - 6 Years Ago
Warren (Staff) - 6 Years Ago
Hanaldo - 6 Years Ago
Robert72 - 6 Years Ago
Hanaldo - 6 Years Ago
Robert72 - 6 Years Ago
Robert72 - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search