First infiusion -fail?


Author
Message
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Ok,I done.first infiusion and I think it's a fail. Resin in cup (left overs )solid,but resin in tubes still soft. I think I made.mistake and I shouldn't take the bag off. I not touch the sheet so might cure till tomorrow.
Any ideas?
Or I should wait another 24hrs next time?
Replies
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Almost certainly; you could put it somewhere warmer or just wait a little longer. As a very rough rule of thumb, a 10'C increase in temperature halves the associated curing times and so a 10'C drop in temperature will double the curing times. Ideally you would maintain at least 20'C for the full curing cycle of the resin but in an unheated workshop/garage at this time of year, it could easily drop well below that. I'd leave it for another 12-24hours before demoulding but see no reason as to why it should have failed, it just needs more time.
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Rich (Staff) - 9/23/2019 2:18:35 PM
Almost certainly; you could put it somewhere warmer or just wait a little longer. As a very rough rule of thumb, a 10'C increase in temperature halves the associated curing times and so a 10'C drop in temperature will double the curing times. Ideally you would maintain at least 20'C for the full curing cycle of the resin but in an unheated workshop/garage at this time of year, it could easily drop well below that. I'd leave it for another 12-24hours before demoulding but see no reason as to why it should have failed, it just needs more time.

It come out quite well.Think to fast infiusion create small air pockets.But the temp. Was the main.issue.I know now if resin is cured in tube it should be fine.๐Ÿ‘