How much
Add Vote
Show Results
Author
Message
kevdickson
k
kevdickson
posted 6 Years Ago
ANSWER
HOT
Poll Details
k
Group: Forum Members
Posts: 1,
Visits: 34
First time user
Having issues on how much pigment to use I am using black so only using 5% but is it 5% of the combined resin and hardener thus being 25 grams of pigment or is it 5% of just the resin weight
I am using a 500 gram kit
Edited
6 Years Ago by
kevdickson
Reply
Like
3
Reply
Warren (Staff)
Warren (Staff)
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Generally speaking, the pigment ratio is a percentage of the entire mix so resin AND hardener.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pigment
kevdickson
-
6 Years Ago
Generally speaking, the pigment ratio is a percentage of the entire mix so resin AND hardener.
Warren (Staff)
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search