By kevdickson - 8/12/2019 8:18:54 PM
First time user Having issues on how much pigment to use I am using black so only using 5% but is it 5% of the combined resin and hardener thus being 25 grams of pigment or is it 5% of just the resin weight
I am using a 500 gram kit
|
By Warren (Staff) - 8/13/2019 8:40:22 AM
Generally speaking, the pigment ratio is a percentage of the entire mix so resin AND hardener.
|
|