Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 133,
Visits: 566
Simply, how to make a mould from a piece covered by leather, without causing damages to it (and to be able to restore it) ?
Any sort of protection to lay up first which would be harmless to the leather, before applying ease-lease release agent, wax, and gel coat ?
thank you for reading me
J
Reply
Like
2
Replies
fgayford
fgayford
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Jess8bit (12/11/2012)
Simply, how to make a mould from a piece covered by leather, without causing damages to it (and to be able to restore it) ?
Any sort of protection to lay up first which would be harmless to the leather, before applying ease-lease release agent, wax, and gel coat ?
thank you for reading me
J
I have made polyester molds over wet clay and over styrofoam. There are 4 ways that you can do this, that has worked for me.
1. I cover the piece with saran wrap. (kitchen wrap the cling kind) carefully gelcoat and lay up your reinforcement when tacky.
2. Tin foil over the piece. I will often spray a little tackifier (3M 77) it get it to stick. Make your mold.
3. Packing tape over the whole piece and then wax. Now make your mold.(it may tear your leather when you release the tape so the above might work better.
4. Use silicone rubber. it will release cleanly and have every detail.
Fred
Reply
Like
3
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
Hi Fred,
thank you so much for sharing !! I would'nt have guessed so many possibilities
Especially I like the kitchen wrap
Best Regards,
Jess.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Making a smooth mould from a leather part.
Jess8bit
-
13 Years Ago
[quote][b]Jess8bit (12/11/2012)[/b][hr]Simply, how to make a mould from a piece covered by leather,...
fgayford
-
13 Years Ago
Hi Fred, thank you so much for sharing !! I would'nt have guessed so many possibilities :)...
Jess8bit
-
13 Years Ago
Kitchen wrap or release film would be your best bet... Thats a good idea and probably how I would do...
baja_patient
-
13 Years Ago
Thank you !
Jess8bit
-
13 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search