Chrome pattern rusty filling before or after?


Author
Message
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
I got chrome bumper 
where on 90% surface chrome is fine,just underneath get bit rusty.
Rust is to big to polish,should I use a filler ?or leave that for.later on and polish the gelcoat?
Thanks

Edited 6 Years Ago by Classicarbon
Replies
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
I'm not certain that Warren picked-up on the fact that you're looking to take a mould from the bumper and thought, perhaps, that you were just looking to fix the rusty areas?

Rattle can paints are unlikely to give you a good surface from which to mould from and it would likely be attacked by the gel coat and come away during de-mould

You might just end up with some rough spots if you went ahead and moulded direct from it as is, but you might also get spots of gel coat sticking to the rusted areas that leave you with holes to repair afterwards in the mould 

If you're not minded to paint the whole thing with a reliable paint system in order to get a good surface all over, you could opt to cover the bad bits with flash tape if that element of the part would be mostly hidden when mounted (underside?). This would be the 'quick and dirty' option but probably depends upon how critical the affected area is to the part cosmetically. If you opt to use ordinary filler this would likely stick and pull away upon de-mould and the process of flatting it would also scratch-up the surrounding areas, so likely not a great option on its own. 




Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
MarkMK - 8/12/2019 4:05:31 PM
I'm not certain that Warren picked-up on the fact that you're looking to take a mould from the bumper and thought, perhaps, that you were just looking to fix the rusty areas?

Rattle can paints are unlikely to give you a good surface from which to mould from and it would likely be attacked by the gel coat and come away during de-mould

You might just end up with some rough spots if you went ahead and moulded direct from it as is, but you might also get spots of gel coat sticking to the rusted areas that leave you with holes to repair afterwards in the mould 

If you're not minded to paint the whole thing with a reliable paint system in order to get a good surface all over, you could opt to cover the bad bits with flash tape if that element of the part would be mostly hidden when mounted (underside?). This would be the 'quick and dirty' option but probably depends upon how critical the affected area is to the part cosmetically. If you opt to use ordinary filler this would likely stick and pull away upon de-mould and the process of flatting it would also scratch-up the surrounding areas, so likely not a great option on its own. 




You right,think the best way might be to clean it as.much as possible,fill it up and smooth it out as much as possible and cover it with flash tape.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Classicarbon - 6 Years Ago
Warren (Staff) - 6 Years Ago
Classicarbon - 6 Years Ago
MarkMK - 6 Years Ago
Classicarbon - 6 Years Ago
Warren (Staff) - 6 Years Ago
             That's me on the right way again. Thanks
Classicarbon - 6 Years Ago
Classicarbon - 6 Years Ago
SleepingAwake - 6 Years Ago
                     So.might use flash tape on the holes only.
Classicarbon - 6 Years Ago
Warren (Staff) - 6 Years Ago