Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Table with easycell core
Table with easycell core
Post Reply
Like
2
Table with easycell core
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
allankn
a
allankn
posted 6 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 8,
Visits: 192
I’m doing a table with easycell core. Quick control question.
Should I infuse the different sides on top of the core separately for best results?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Table with easycell core
allankn
-
6 Years Ago
It is possible to infuse with Easycell foam sheet but you'd need to make small holes at around 50mm centres in the sheet thicknesses below 10mm in order to do it in one go. This, however, will leave....
MarkMK
-
6 Years Ago
Thanks, appreciate it!I will not ask ;)
allankn
-
6 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search