Hi,

Can your Epoxy Coating Resin be sprayed with a spray gun?

If affirmative, what nozzle should i use? 2,5mm?

Pedro
Replies
pedcrist
pedcrist
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 42, Visits: 350
Thats my ideia.

I´m going to research lacquer to apply.

Thanks, Matt.

Pedro
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
pedcrist (13/11/2012)
Thats my ideia.

I´m going to research lacquer to apply.

Thanks, Matt.

Pedro


Hi Pedro

I spray 2k in the mold first and then infuse next day. It works great.

Fred 