Epoxy Coating Resin can be sprayed?


Author
Message
pedcrist
pedcrist
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 42, Visits: 350
Hi,

Can your Epoxy Coating Resin be sprayed with a spray gun?

If affirmative, what nozzle should i use? 2,5mm?

Pedro
Replies
pedcrist
pedcrist
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 42, Visits: 350
Hi, Matt

Thanks for your quick anwser.

My intention to spraying the clear coat is to get the pieces to be finished right after the resin cures.

If the resin is brushed, have to be sanded and polished.

Using the gelcoat spray gun to apply the resin, with the #6 nozzle(4.7mm), it will be smooth, or it will be irregular and i´ve got to sand/polish it too?

Pedro
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Pedro,

If your plan is to use the Epoxy Coating Resin as a sort of clear coat then you would be much better off actually using clear coat (lacquer). I would recommend a 2k PU or acrylic lacquer, sprayed through a normal gun. This will give you a better clear finish than spraying the epoxy coating resin and will provide UV stability too.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search