Hi,

Can your Epoxy Coating Resin be sprayed with a spray gun?

If affirmative, what nozzle should i use? 2,5mm?

Pedro
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Pedro,

Although I've never tried it I wouldn't suggest spraying the coating resin if you're using the resin clear and coating something where the clarity (particulary in terms of air entrapment)  is important. The reason is because it's a very viscous resin and it's so important when coating with clear epoxy to reduce the chances of air entrapment wherever possible, I would be worried that spraying might cause air entrapment.

If you do spray, you'll need something larger like 4mm+ nozzle, given how thick this coating resin is.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search