Group: Forum Members
Posts: 460,
Visits: 5.2K
|
I used to simulate and run AFP machined and we have some new hybrid twchnology being installed at work. You should be able to gather some results via Google academia searching for AFP process parameters.
Also search for people, m Torres, electroimpact, ingersoll and cincinnati ago machines there is documents online.
There aren't many books available if any, most of the knowledge is retained within the companies producing and using the machines.
|