Hi,
Im building a model boat,im going to use pre peg carbon and aramid honey comb ,I want to reinforce some areas using Kevlar but theres no pre peg Kevlar only fabric,
how can i do this,is it possible?

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Without the availability of a co-curable aramid based pre-preg, you would need to laminate the aramid as a separate stage. Once the pre-preg has cured, if you haven't peel ply'd the bonding area, give it a good key with 120 grit paper then wet lay laminate the kevlar into place.  I would recommend choosing a resin suitable for your intended service temperature and then carry out a full post cure on it before moving on to the assembly of the sandwich panel. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Fasta
Fasta
Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)Supreme Being (6.7K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
If the kevlar is the very light 60g dry fabric (without resin) then this would be light enough to just place against the a layer of pre preg carbon and there is very likely enough resin there to wet that out too.




f1rob
f1rob
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
carlton jacobs - 7/17/2019 3:07:49 PM
Hi,
Im building a model boat,im going to use pre peg carbon and aramid honey comb ,I want to reinforce some areas using Kevlar but theres no pre peg Kevlar only fabric,
how can i do this,is it possible?

There's plenty of pre preg kevlar about
Both in yellow an pigmented black 
Probably SHD is your best bet to get it in small amounts